SA-213/SA-213M Specification for seamless Ferritic Alloy steel boiler, Superheater and heat exchanger tubes Delivery Condition: Normalized and Tempered Inspections and Tests Performed: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength, Yield Strength, Elongation,...

 

SA-213/SA-213M Specification for seamless Ferritic Alloy steel boiler, Superheater and heat exchanger tubes

Delivery Condition: Normalized and Tempered
Inspections and Tests Performed: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength, Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test, No-destructive Test, Hydrostatic Test.
Surface treatment: Oil-dip, Varnish, Passivation, Phosphating, Shot Blasting 
Inner packing: Caps on two ends of every pipe 
Package: bare packing/bundle packing/wooden carton packing.

Size Tolerance

Tube Kinds

SA213 OD(D)

SA213 Thickness(S)

OD(mm)

OD Tolerance(mm)

OD(mm)

Thickness Tolerance(mm)

Hot Rolled

≤101.6

+0.4~-0.8

76~168.3

+28%~0

>101.6~168.3

+0.4~-1.2

Cold Drawn

<25.4

0.1

≤38.1

+20%~0

25.4~38.1

0.15

>38.1~<50.8

0.2

>38.1

+22%~0

50.8~<63.5

0.25

63.5~<76.2

0.3

76.2~101.6

0.38

>101.6~190.5

+0.38~-0.64

>190.5~228.6

+0.38~-1.14

 

Grade

Tensile Strength,Min., ksi[MPa]

Yield Strength,Min., ksi[MPa]

Elongation
in 2 in. or 50 mm,Min., %[Note (1),(2)]

T12

60 [415]

32 [220]

30

T23

74 [510]

58 [400]

20

T91

85 [585]

60 [415]

20

T92

90 [620]

64 [440]

20

T122

90 [620]

58 [400]

20

18Cr-2Mo

60 [415]

40 [275]

20

NOTES:
(1) When standard round 2 in. or 50 mm gage length or smaller proportionally sized specimens with gage length equal to 4D (4 times the diameter) is used, the minimum elongation shall be 22% for all ferritic grades except 18Cr-2Mo, T23 and T91.
(2) For longitudinal strip tests, a deduction from the basic minimum

 

CHEMICAL REQUIREMENTS FOR FERRITIC STEEL

Composition, %

Grade

Carbon

Manganese

Phosphorus, Max.

Sulfur, Max

 Silicon

Chromium

Molybdenum

Titanium

Vanadium,Min.

Other Elements

T2 [Note (1)]

0.10–0.20

0.30–0.61

0.025

0.025

0.10–0.30

 0.50–0.81

 0.44–0.65

 . . .

 . . .


T5

0.15 max.

0.30–0.60

0.025

0.025

0.50 max.

4.00–6.00

0.45–0.65

. . .

. . .


T5b

0.15 max.

0.30–0.60

0.025

0.025

1.00–2.00

4.00–6.00

0.45–0.65

 . . .

. . .


T5c

0.12 max.

0.30–0.60

0.025

0.025

0.50 max.

4.00–6.00

0.45–0.65

[Note (1)]

 . . .


T9

0.15 max.

0.30–0.60

0.025

0.025

0.25–1.00

8.00–10.00

0.90–1.10

. . .

. . .


T11

0.05 min.–0.15 max.

0.30–0.60

0.025

0.025

0.50–1.00

1.00–1.50

0.44–0.65

 . . .

. . .


T12 [Note (1)]

0.05 min.–0.15 max.

0.30–0.61

0.025

0.025

0.50 max.

0.80–1.25

0.44–0.65

. . .

. . .


T17

0.15–0.25

0.30–0.61

0.025

0.025

0.15–0.35

0.80–1.25

. . .

 . . .

0.15


T21

0.05 min.–0.15 max.

 0.30–0.60

0.025

0.025

0.50 max.

2.65–3.35

0.80–1.06

 . . .

. . .


T22

0.05 min.–0.15 max.

0.30–0.60

0.025

0.025

0.50 max.

1.90–2.60

0.87–1.13

. . .

 . . .


T23

0.04–0.10

0.10–0.60

0.03

0.01

0.50 max.

1.90–2.60

0.05–0.30

 . . .

0.20–0.30

W 1.45–1.75
     Cb 0.02–0.08
     B 0.0005–0.006
     N 0.030 max.
     Al 0.030 max.

T91

0.08–0.12

0.30–0.60

0.02

0.01

0.20–0.50

8.00–9.50

0.85–1.05

. . .

0.18–0.25

Cb 0.06–0.1
     N 0.030–0.070
     Ni 0.40 max.
     Al 0.04 max.

T92

0.07–0.13

0.30–0.60

0.02

0.01

0.50 max.

8.50–9.50

0.30–0.60

. . .

0.15–0.25

W 1.5–2.00
     Cb 0.04–0.09
     B 0.001–0.006
     N 0.03–0.07
     Ni 0.40 max.
     Al 0.04 max.

T122

0.07–0.14

0.70 max.

0.02

0.01

0.50 max.

10.00–12.50

0.25–0.60

. . .

0.15–0.30

W 1.50–2.50
     Cu 0.30–1.70
     Cb 0.04–0.10
     B 0.0005–0.005
     N 0.040–0.100
     Ni 0.50 max.
     Al 0.040 max.

18Cr-2Mo

0.025 max.

1.00 max.

0.04

0.03

1.00 max.

17.5–19.5

1.75–2.50

[Note (3)]

 . . .

N max. 0.035
     Ni + Cu max. 1.00

NOTES:
(1) It is permissible to order T2 and T12 with 0.045 max. Sulfur.
(2) Grade T5c shall have a titanium content of not less than four times the carbon content and not more than 0.70%.
(3) Grade 18Cr-2Mo shall have Ti + Cb p 0.20 + 4 (C + N) min., 0.80 max.

 

 

SUNRISE is well-known as one of the leading asme sa213a213 seamless alloy steel boiler super heater and stainless steel heat exchanger tubes manufacturers and suppliers in China for its quality products and excellent service. We warmly welcome you to buy the quality and durable steel products from our factory.